Hello,

could someone tell me the ANSI or ISO designations for these two steel compositions:

C Si Mn P S Cr
0.30 0.25 0.50 0.035 0.040 0.95

C Si Mn P S Cr Ni Pb
0.98 0.23 0.46 0.014 0.050 0.15 0.06 0.19

Thanks
Pete
 
Replies continue below

Recommended for you

The first composition is similar to grade 5132 according to SAE J404, but the Mn is to low; it should be 0.60-0.80. Grade 34Cr4 appears in ISO standards like 4954 and EN standards like EN 10263-4 is equivalent to the 5132 and likewise has a minimum Mn content of 0.60.

The second composition meets the requirements of 10L95 according to SAE J403. C100S acording to EN 10132-4 is a nominally 1% C steel for spring discs, but the maximum S content is 0.035 and there is no Pb. C98D2 according to EN 10016-4 is another ~ 1% C steel for drawn wire, and it is common in Europe to specify something like C98D2 + Pb to make it a "free-machining" version of a standard steel.
 