We usually performe chemical cleanings to some equipments, like pumpes, piping, vessels, in a closed circuit usually with citric or phosphoric acid. I was told that the best way to know when to stop the cleaning (if visual inspection is not possible) was to do some total iron analysis. Is this true? If so, how does the iron chart looks like?
Thank you
DL
Thank you
DL