Hello everybody:

For the manufacture of the penstock (Ø 1,2 m) for a mini hydropower plant, it was specified to use steel ASTM A 560 Gr 60. The representative of the client is requesting to use steel API 5LX70.

Regardless of the prices or the calculations of the required plate thickness, is it technically correct to achieve that substitution? Are these steels interchangeables?

Any received information on this subject will be highly appreciated.
 
Replies continue below

Recommended for you

Neither spec is interchangeable, in fact quite different things entirely. One is a spec for steel castings, the other is a spec for pipe! One is high strength normal temperature ,low carbon steel, the other is high strength, high temperature, high alloy chrome, stainless and I wouldn't think you'd need that in a penstock, so what gives?

Let your acquaintances be many, but your advisors one in a thousand’ ... Book of Ecclesiasticus
 
Hello everybody:

Thanks BigInch for your comment.
 