Hello everybody:
For the manufacture of the penstock (Ø 1,2 m) for a mini hydropower plant, it was specified to use steel ASTM A 560 Gr 60. The representative of the client is requesting to use steel API 5LX70.
Regardless of the prices or the calculations of the required plate thickness, is it technically correct to achieve that substitution? Are these steels interchangeables?
Any received information on this subject will be highly appreciated.
For the manufacture of the penstock (Ø 1,2 m) for a mini hydropower plant, it was specified to use steel ASTM A 560 Gr 60. The representative of the client is requesting to use steel API 5LX70.
Regardless of the prices or the calculations of the required plate thickness, is it technically correct to achieve that substitution? Are these steels interchangeables?