Hello,

I am working on a heat exchanger that has a shell made of steel 15 366. I need to weld the shell as a temporary measure. But, I have no idea what steel 15 366 is. I cannot find its specification under any standard. I will be doing TIG welding but I still cannot figure out the reloading/filling material.