The frequency of our FCCU Wet Gas Compressor turbine fouling has increased sharply this year. We have conducted an online cleaning three times this year compared to two times last year. Please note that in Year 2001 we only cleaned it ONE time.
Does any body has/ had experience such a problem and what the action that has been taken to avoid such problem. It is really hearting us by reducing feed and severity for two shifts which then will impact on our profitability.
I appreciate your assistance and help in this matter. Tks