You should review ASTM A193 to make sure which Class you want (probably Class 1). You can order the initial bar as Type 316 according to ASTM A276, but you have to make sure you also require the bar plus final parts to meet ASTM A193, Grade B8M, Class _, where you decide which class is appropriate.