Dec 23, 2009 #1 M MintJulep Mechanical Jun 12, 2003 10,162 Can anyone point me to metric standards for prevailing torque fasteners equivalent to: MS-21044 or MIL-N-25027 for nylon insert nuts and MIL-DTL-18240 for nylon plug and strip external thread fasteners?
Can anyone point me to metric standards for prevailing torque fasteners equivalent to: MS-21044 or MIL-N-25027 for nylon insert nuts and MIL-DTL-18240 for nylon plug and strip external thread fasteners?
Dec 23, 2009 #2 CoryPad Materials Apr 15, 2002 5,192 I can't speak to equivalency, but the only standards for these types of parts that I am aware of are the IFI 5XX series. You can search here: http://www.indfast.org Upvote 0 Downvote
I can't speak to equivalency, but the only standards for these types of parts that I am aware of are the IFI 5XX series. You can search here: http://www.indfast.org
Dec 23, 2009 #3 TVP Materials Apr 12, 2002 4,592 ISO 7040 and 10513 are two metric standards for nylon prevailing torque nuts. Upvote 0 Downvote