dcarr82775
Structural
ACI318 allows for a reduction in the 'ldh' with a standard hook for the ratio "As req'd/As provided". I have a situation where I have a standard hooked bar, but the length of the hook is only about 11 bar diameters instead of 12 bar diameters. It would take too long to explain how this happened but the concrete is already cast.
ACI doesn't address this condition, but I wanted to see if others thought a similar reduction ratio (91%=11/12) on the bar strength is a reasonable approach? If the hook was drastically shorter I don't think I would look at this approach but for something this close I do not think it is too far out in left field.
ACI doesn't address this condition, but I wanted to see if others thought a similar reduction ratio (91%=11/12) on the bar strength is a reasonable approach? If the hook was drastically shorter I don't think I would look at this approach but for something this close I do not think it is too far out in left field.