May 23, 2002 #1 Adrian2 Mechanical Joined Mar 13, 2002 Messages 303 Location CA Dear Folks; Does anyone have a list or a link to standard gauges for bolt placement in angles and channels in english units. My Canadian Steelbook shows only metric. Regards Adrian
Dear Folks; Does anyone have a list or a link to standard gauges for bolt placement in angles and channels in english units. My Canadian Steelbook shows only metric. Regards Adrian
May 23, 2002 1 #2 Mattman Structural Joined Jul 20, 2001 Messages 64 Location US From AISC ASD 9th, Page 1-52: Leg 8 7 6 5 4 3.5 3 g 4.5 4 3.5 3 2.5 2 1.75 g1 3 2.5 2.25 2 g2 3 3 2.5 1.75 Leg 2.5 2 1.75 1.5 1.375 1.25 1 g 1.375 1.125 1 0.875 0.875 0.75 0.625 Upvote 0 Downvote