NDTLevel3

Materials
Sep 30, 2000
24
Does anyone know of a standard or spec which describes this process? We are looking for grinding burns.

Thanks,

Bill

William E. Blum
Manager
NDT Consulting Group Inc.
wblum@ndt-cgi.com
USA 1-877-638-2441
Fax/Voice Mail 1-214-853-5131
Sweden 46-42-14 39 99
 
Replies continue below

Recommended for you

I know there are a number of standards for acid etch inspections, such as AMS-2649, MIL-STD-867 or ANSI B3.3 - I'm not sure if they specifically address high temp steels. They may be a starting point....
 