We purchase many materials ranging from A36 structural steels to AA304, ss316, ss430 rods. These materials are received sometimes with stamping of heat numbers and sometimes without stamping and only with MTC. In these cases we are immediately trasfering the HT in the MTC on to the materials.
Can we continue this process. Kindly suggest
 