- what is the difference between 304H stainless steel and 304 stainless steel ?as I know the grain size of 304H shall be coarser than ASTM No.7. but all of the mechanical properties of these two kind of steels are the same.
- can we use 304ss instead of 316ss at 550 centigrade degree?
316ss has additional element such as Mo which is effective for creep resistance,but base on ASME SecII partD the maximum temperature for 304ss is 1500F and for 316ss is 800F.
- can we use 304ss instead of 316ss at 550 centigrade degree?