I've seen somewhere on the web that an organization (I believe AISC) is coming out with a design guide or specification for Stainless Steel design. Anyone know what's going on with this.
 
Replies continue below

Recommended for you

There are good books on this subject.
I haven't seen any web activity that was nearly thorough enough to be useful.
Start with this one from ASM:

Stainless Steels for Design Engineers

Author(s): Michael F. McGuire
Audience This book gives engineers and designers a valuable guide on stainless steels and how to use them.Easy to read, this helpful technical guide is for anyone who designs or builds with stainless steels.
Hardcover
05231G
In Stock
Price $179.00
Member Price $129.00

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Eurocode 3 (EN 1993) already covers stainless steel for structures.
 
ASCE Standard 8-02 covers Specification for the Design of Cold-Formed Stainless Steel Structural Members. This was originally produced by AISI then ASCE took it over.
 
I agree with CoryPad, Eurocode 3 already covers stainless steel.
Moreover, the Steel Construction Institute (SCI) has also published a design guide about stainless steel which is really useful. It contains a lot of theoretical information as well as design examples.

All about Eurocodes:
 