I have a chart of pipe properties that indicates that the thickest 14" pipe for ss is 10S. The chart references ANSI B36.19 stainless steel pipe schedule numbers.
I have been told by our field services that stainless steel pipe can be purchased in sch 40S with no problem.
If this is true, why does the chart not show that sch40S is available????
TIA
I have been told by our field services that stainless steel pipe can be purchased in sch 40S with no problem.
If this is true, why does the chart not show that sch40S is available????