bunyer

Automotive
Jun 6, 2005
7
Does anybody have any experience of using SS304 matl for a banjo bolt?
 
Replies continue below

Recommended for you

Might be a bit soft, though a work hardened grade might be available. I would definately check the tensile stresses in the bolt vs the strength of the banjo. If the force required to seat the copper sealing washers is greater than that required to stretch the bolt, the bajo fitting wont seal.
 
Too soft, check with McMaster-Carr or Aircraft Spruce for some 17-4 or similar.
 
If you are concerned about dis-assembly, a good coat of anti-sieze goes a long way.
 
If you are concerned about dis-assembly, a good coat of anti-sieze goes a long way.

SS fasteners can foul just as easily on assembly as disassembly...I never assemble SS cap screws without some form of lube, never! In some applications where lubricant may interact with the product, O2 etc., several forms of wax can be used.

SS banjo bolt? I don't see a problem as torque is not an issue in most cases---copper or aluminum sealing washers are rather soft. I do see one issue, that of loosening in vibration service. Not a common problem but, none the less...a chemical locking agent would cure the problem as well as lube the assembly, but dissambly could be a problem.

Rod

 
If you check out manufacturers like Goodridge and Hel who make braided brake lines for motorcycles etc you will see that stainless is used. One company even quoted using 303.
 