Hello,
I am having some trouble with 316L stainless steel cracking when i want to flatten it into an oval shape. I want to fit 2 nitinol wires into the oval shape and crimp them without the 316L ss cracking. Would annealing and flattening them to oval help considerably with the cracking? Is there any services to make the 316L ss more malleable? I'm also trying to look for services from companies that would do something like this. I have a drawing attached.
Thanks
I am having some trouble with 316L stainless steel cracking when i want to flatten it into an oval shape. I want to fit 2 nitinol wires into the oval shape and crimp them without the 316L ss cracking. Would annealing and flattening them to oval help considerably with the cracking? Is there any services to make the 316L ss more malleable? I'm also trying to look for services from companies that would do something like this. I have a drawing attached.