Can anyone explain the circumstances in which PWHT of 321 SS is appropriate? A customer has recently asked my shop to prepare a WPS for welding SA-312 TP321 pipe to itself and apply 1100 deg F PWHT for 1 hour. This seems like a recipie for carbide precipitation to me. The base metal thickness is 0.432", welded with GTA root and SMA fill and cap, using 321 rod. My stainless weld prcoedures are usually designed to keep the heat input as low as possible and keep the interpass temp are 375 F. The customers primary concern seems to be ductility in the as-welded condition, but I believe the proposed "cure" is going to make things worse.