Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Stainless fasteners in carbon steel - wet environment 1

Status
Not open for further replies.

CrazyJ

Mechanical
Joined
Feb 23, 2003
Messages
12
Location
CA
I've installed equipment where the supplier gave 8.8 bolting for carbon steel to carbon steel. The application is wet. Now I know enough to say that A2-70 and A2-80 are not quite up to the yield strength of an 8.8 fastener. However, I'd like to change out the fasteners to stainless steel, but is there any benefit here? If we paint them, is there any benefit to installing a stainless fastener in this application?

I would worry enough about the yield strength in this application to say the new fastener would need at least equivalent, or very close.

I see that B6 threaded rod is roughly equivalent, but why is there so little information on B6, where B7 and B8 seem to get 'all the press'. Is there some application where all they use is B7 or B8?
 
Hi crazyJ

I'd be concerned about galvanic corrosion between stainless and carbon steel.

desertfox
 
You may be better off just using coated CS bolts. There are many sources for good coated bolts.

= = = = = = = = = = = = = = = = = = = =