Jan 18, 2016 #1 meetsangrealhere Mechanical Joined Jan 18, 2016 Messages 1 Location AE i would like to know, whether SSC test been carried for A625 grade materials. kindly specify what all test can be done on A625 ?
i would like to know, whether SSC test been carried for A625 grade materials. kindly specify what all test can be done on A625 ?