hi
For forged Stainless steel fittings and flanges which meet NACE MR175 requirements, is SSC test mandatory for these material? if yes or no, please specify the clause of the standard.
 
Replies continue below

Recommended for you

Why not read through the standard and conclude for yourself? When you say 'meets NACE MR(0)175 requirements,' do you mean that you have also confirmed the environment to which the material will be exposed to and found it acceptable?

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
What type of stainless steel, i.e. austenitic, martensitic, etc.?
 