We have an assy using a solid 5" bar of 316L with 24" dia x 3/8" thick flanges welded at 18" intervals. I need to look at suitable SN data for 316L but cannot locate any in my available sources. Any ideas where to find data?
 
I'm sure there is a lot of fatigue testing data around, but you need to be aware that the fatigue strength of annealed 304/316 SS is very low. I am aware of failures where the calculated stresses varied only +/- 7 ksi!
 
The Handbook of Stainless Steel gives the endurance limit for 316 as 39 ksi based on data from INCO. This is for reversed bending.
 
Extensive fatigue information can be found in the "Aerospace Structural Metals Handbook".