I was asked about corrosion resistant springs for a boat trailer used on the Texas coast.These trailers are backed into the water to launch and have to be replaced in a few years .Is there a SS that would do better ? I did some jobs years ago, 1970s, on Padre Island and there you didn't have to dunk things into water the high moisture/salt/temperature did a great job on everything !Retired now I'm somewhat out of the loop .Anything available in newer SS ?
 
Replies continue below

Recommended for you

Yes, Springflex by Sandvik. It is a 22 % Cr alloy with a PRE of 35 so that it has substantial resistance to chloride environments.



Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
I would think that 2205 might be an option. The high strength would be nice also. I would have to think about fatigue limit, I am not sure off of the top of my head.

= = = = = = = = = = = = = = = = = = = =