We have the second of our Ozone plants on line. The plants are processing / using the same source water.
This is all well and good but on the second plant on - stream we seem to be experiencing through the weld leaks.
The pipes in question operate at ~ ~ 4 p H.
We have not had problems with the first plant and this has
been a real curve ball -
We have about 40 joints leaking and this is totally new to
my experience as I have worked with austenitic stainless
in ASME Section VIII and Piping and have not experienced this since 1968 -
Has anyone experienced anything similar ? ? ?
This is all well and good but on the second plant on - stream we seem to be experiencing through the weld leaks.
The pipes in question operate at ~ ~ 4 p H.
We have not had problems with the first plant and this has
been a real curve ball -
We have about 40 joints leaking and this is totally new to
my experience as I have worked with austenitic stainless
in ASME Section VIII and Piping and have not experienced this since 1968 -
Has anyone experienced anything similar ? ? ?