SS 304L for NITRIC ACID(68%STRENGTH) 1

Status
Not open for further replies.

dkbheda

Mechanical
Joined
Jul 6, 2002
Messages
3
Location
IN
Hello Gentlemen,

Can we store Nitric Acid (68%) in carbon steel tank internally cladded with Stainless steel grade SS 304 L 2mm thk sheeting?what will be the corrosion rate?

I welcome your views on the same.

dilip
 
304L will do fine. Sedricks ( Corrosion of Stainless Steel) gives the corrosion rate at less than 0.005 inch/year at 90C. At room temperature, there's not anything measurable to worry about.
 
Schweitzer says less than 0.002 inches per year at room temperature.
 