Can we store Nitric Acid (68%) in carbon steel tank internally cladded with Stainless steel grade SS 304 L 2mm thk sheeting?what will be the corrosion rate?
304L will do fine. Sedricks ( Corrosion of Stainless Steel) gives the corrosion rate at less than 0.005 inch/year at 90C. At room temperature, there's not anything measurable to worry about.