has any one tested 204Cu stainless steel behavior in seawater?
 
Replies continue below

Recommended for you

SS 204Cu was developed has a cheaper alternative to SS 304 as you can read in this articles and has, more or less, the same corrosion resistance of SS 304. SS 304 is not recommended for service in SeaWater due to the very low corrosion resistance, low pitting and crevice temperature.

DEVELOPMENT OF TYPE 204 CU STAINLESS,A LOW-COST ALTERNATE TO TYPE 304



hope this help

S

Corrosion Prevention & Corrosion Control
 
Adding to strider6's informative post there is always the problem with stress cracking in the form of Stress Corrosion Cracking".
 