Oct 18, 2007 #1 Kresimir Petroleum Joined Mar 21, 2005 Messages 7 What is the optimum inlet temperature for the TGTU hydrogenation reactor (CoMo catalyst), to ensure maximum conversion of S, SO2, COS CS2 into H2S?
What is the optimum inlet temperature for the TGTU hydrogenation reactor (CoMo catalyst), to ensure maximum conversion of S, SO2, COS CS2 into H2S?
Oct 18, 2007 #2 25362 Chemical Joined Jan 5, 2003 Messages 4,826 Location CA See page 5+ in http://www.criterioncatalysts.com/english/PDF/SNM-Tailgas-2-26-01.PDF Upvote 0 Downvote