Hi Experts,
Now we are dealing with this issue: High frequency noise from the vehicle exhaust rear hanger due to the engine movement.
The root caise is the friction between rubber of the hanger and the steel of the rod. A stick & slip phenomenon happens providing the noise.
We are now testing a lubricated rubber proposed by a supplier and it works. But this rubber has also different geometry.
Do you have some experience in this cases?
Would you propose some technical meterial regarding lubrified rubbers?
Now we are dealing with this issue: High frequency noise from the vehicle exhaust rear hanger due to the engine movement.
The root caise is the friction between rubber of the hanger and the steel of the rod. A stick & slip phenomenon happens providing the noise.
We are now testing a lubricated rubber proposed by a supplier and it works. But this rubber has also different geometry.
Do you have some experience in this cases?
Would you propose some technical meterial regarding lubrified rubbers?