Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations 3DDave on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Springs - Distempered or Detempered

Status
Not open for further replies.

Lakey

Electrical
Jul 25, 2003
66
Hi Folks,

I have a compression spring that has been affect by heat.

Is it correct to say that the spring has been "distempered" or is it more correct to say "de-tempered"?

I would appreciate your comments.

Regards,

 
Replies continue below

Recommended for you

My personal view is that it is correct to say “de-tempered”, but I’ve had a conflicting opinion. Hence I want to check.
 
I would say, "the spring lost it's temper."
 
I think Distemper is a disease common in dogs. :)
 
Depending on the time/temperature it has experienced I think the correct terms may be annealed, normalized, or stress relieved.
 
It depends on the type of spring wire used.If a tempered wire product was used (e.g.oil tempered or chrome silicon) then Carburize's description is spot on. But, if the wire was music wire, stainless or something else, then some other term might be more appropriate.
 
How about overheated? Unless the temperature was in excess of ~ 650 C, then annealed does not apply. If the temperature did not exceed the A3 temperature (> 730 C), then normalized does not apply.
 