hi,
I need information about the effect of spray water pressure on the solidification profile in the secondary cooling zone of continuous casing of steel
 
Replies continue below

Recommended for you

metudgn;
During my audits of various tube mills, I have seen software that is used to predict solidification affects of continuous cast strands that are eventually used to make pipe and tube products for Power Generation use. Why are you asking this question?
 
metudgn,

Have you performed a keyword search using an appropriate search engine like Compendex, CSA from ProQuest, Scirus, or Google Scholar? Do you have an adversarial relationship with the vendor that manufactured your caster?
 