Bridgeman44
Structural
I'm working on a rehabilitation project for significantly deteriorated corrugated structural plate pipe arches. They are dual culverts with 2' space between them and they are about 7'-6" wide x 5'-3" high. There is only about 1 ft cover over them with a 2-lane roadway above. I'm just trying to find out what people are using these days to rehab these pipe arches and what seems to work best for the least money of course! The deterioration is mainly the bottom exhibiting significant section loss and perforations throughout, some very large. There are also some minor to moderate (say intermittent over 5 linear feet) areas of section loss and smaller perforations along the top. I've see lots of these that have been repaired by using a paved concrete invert, but that's about it. I'm interested in any suggestions people might have, thanks!!