datsun280zman
Materials
I`ve got a spot welder I`m trying to use for thin stainless sheet. (.020") Problem is, it`s way too powerful and there`s no adjustment. I`ve been looking at some way of toning down the power and was wondering if I can use a variable speed control device for controlling the input voltage. The welder is a 110v AC. Would this work?
The owners manual that came with it stated that for that gauge of steel the switch should have to be depressed for 2-4 seconds. I can`t hold the switch for more than 1/4 sec without blowing holes through both pieces!
Any help appreciated.
The owners manual that came with it stated that for that gauge of steel the switch should have to be depressed for 2-4 seconds. I can`t hold the switch for more than 1/4 sec without blowing holes through both pieces!
Any help appreciated.