I have a contractor who is replacing a portion of our houses' sill plate due to dry rot of the existing joist. The floor joists are split in the center and some are not even nailed to the sill plate and they are completely missing the rim joists. Contractor stated not his problem. Can some one direct me to the the code in the California Residential Code or CBC that states wood should be free of cracking. While its obvious this is wrong, I want to throw a code at him and the city inspector. See attached picture. Thanks