Does anybody know how do they grind the internal teeth on small spline gauges? I'm looking at a DIN5480 gage with internal teeth, and the certificate says the errors are in 2 mikrometers, it looks like ground. But how can that be possible. Just out of curiosity...
 
Replies continue below

Recommended for you

wire cut then lapped

also there are special custom made miniture internal arms with a grinding wheel if the spline is large enough fot it to fit.
driven by means of a belt.
 