Apr 30, 2003 #1 seanmc Mechanical Joined Sep 2, 2001 Messages 9 Location AU Does anyone have any experience with spiral wound stainless steel piping in a heavy industrial/ water treatment application. I am told it is significantly cheaper than 316L for example but are there any limitations on its use?