Murali-1311
Mechanical
I'm looking for justification to convince the client for accepting Spiral wound gasket(ASME B16.20)-with SS316 windings/Graphite filler, SS316 inner & outer ring in place of actual project requirement SS304.
Client is reluctant to accept changes even after explaining that SS316 fulfills all requirements of SS304 moreover it is a superior grade with higher corrosion resistance due to added molybdenum. Please suggest possible ways to convince the client.
Client is reluctant to accept changes even after explaining that SS316 fulfills all requirements of SS304 moreover it is a superior grade with higher corrosion resistance due to added molybdenum. Please suggest possible ways to convince the client.