i am again tasked to review the applicability of spiral welded pipes (swp) to our system as these swp's are cheaper than our requirements, which are seamless and/or single longitudinal welded pipes.
consider our design parameters (depending on the fluid):
-6.60 mpag at 282degC;
-7.72 mpag at 294degc;
-2.14 mpag at 216degC;
-1.72 mpag at 208degC;
-1.08 mpag at 183degC;
-3.15 mpag at 222degC;
-3.86 mpag at 198degC;
-3.31 mpag at 198degC and
-1.38mpag at 198degC.
from my surfing some websites, swp's are mainly used for piles, supports, water ducts and the like. there is no mention (or did i miss a website??) that swp's can be used for high pressure, high temperature applications.
can somebody please direct me to a website where a plant uses swp's similar to our applications?
if a plant is authorized to use the api 5L monogram, is it safe to assume that the plant does not manufacture swp's?
is the power piping code b311 applicable also to swp's? does the b311 allow the use of swp's?
can i recommend the use of spiral welded pipes in our application? note that we usually have stub ins, pipe shoes that might compromise the spiral welds. or will such connections have an effect on the integrity of the spiral welds?
thanks and am looking forward to your advices and comments.
consider our design parameters (depending on the fluid):
-6.60 mpag at 282degC;
-7.72 mpag at 294degc;
-2.14 mpag at 216degC;
-1.72 mpag at 208degC;
-1.08 mpag at 183degC;
-3.15 mpag at 222degC;
-3.86 mpag at 198degC;
-3.31 mpag at 198degC and
-1.38mpag at 198degC.
from my surfing some websites, swp's are mainly used for piles, supports, water ducts and the like. there is no mention (or did i miss a website??) that swp's can be used for high pressure, high temperature applications.
can somebody please direct me to a website where a plant uses swp's similar to our applications?
if a plant is authorized to use the api 5L monogram, is it safe to assume that the plant does not manufacture swp's?
is the power piping code b311 applicable also to swp's? does the b311 allow the use of swp's?
can i recommend the use of spiral welded pipes in our application? note that we usually have stub ins, pipe shoes that might compromise the spiral welds. or will such connections have an effect on the integrity of the spiral welds?
thanks and am looking forward to your advices and comments.