Can anyone direct me to a manufacturer of spherical ceramic products?
Thank you.
 
ceramic balls on google or yahoo.

Helps if you know the application and / or material.

In my experience (and depending on what you mean by ceramic)I start with Coors.

Tom

Thomas J. Walz
Carbide Processors, Inc.
 
Sorry, should have been more specific. Would
be an alumino-silicate ceramic along the lines of a well proppant.
Any thoughts?
 
Thanks for the suggestion. I don't think they have the prilling or rotary kiln equipment but I will touch base with them to see if its possible.
 
An oil well proppant is pumped down oil wells to keep cracks underground open so that oil can flow to the well more freely. It needs little pricision in size but has to be cheap. There are companies that make it from fly-ash but I'm not in that business. A google search would seem to be appropriate, or ask the question in the petroleum production forum.
 
you can reach for the ceramic ball valve. Hope this website will be your solution. Or you can email to andybear513@hotmail.com for the electronic brochure of ceramic ball valve (material:zirconia+alumina ceramic)
 