Can I use a spectacle blind of material ASTM A182 F304L instead of ASTM A240-304?

What is the criteria for evaluation of the possibility?
 
Replies continue below

Recommended for you

I suggest: Run the calcs and make the determination for yourself.

 
As per my knowledge, A182 being forged will be a good option. However I am not sure about F304L grade. Is it okay to Choose F304L over F304?
 
304 typically comes in dual certified as 304/304L. I believe it hard nowadays to get straight grades.
 