Hello,

I was looking for some specifications of X 10 CrNiTi 18 10 or X 10 Ni Cr Al Ti 32 21 on the net but found nothing about it.

I need especially the weight of them for m².

Thanks a lot,
 
Replies continue below

Recommended for you

Mass is a volumetric property, so the mass must be specified per cubic meter, not per square meter, unless you fix one of the dimensions. For your alloys, the mass density is near 7 900 kg m-3.

Regards,

Cory