DIN 931 is hex bolt with shaft.Replaced by ISO 4014
DIN 933 is hex bolt full thread.Replaced by ISO 4017.

Above standards only show dimensions.
The 10.9 is the material type.See ISO 898-1 Tensile 1000MPa, Yield 900 MPa.
10.9 is also found in ASTM A490
 