Jun 26, 2007 #1 metmama Materials Joined Jun 26, 2007 Messages 1 Location US What are the ASTM/ASME specification numbers for 2.25Cr-1Mo-0.25V pressure vessel steel for heavy wall reactors?
What are the ASTM/ASME specification numbers for 2.25Cr-1Mo-0.25V pressure vessel steel for heavy wall reactors?
Jun 26, 2007 #2 EdStainless Materials Joined May 20, 2004 Messages 16,349 Location Waukesha WI USA I suppose this is 22V, K31835. It is covered by ASME SA-336, 541, 542 and 832. Look them up and which scope covers your product size. = = = = = = = = = = = = = = = = = = = = Rust never sleeps Neither should your protection http://www.trent-tube.com/contact/Tech_Assist.cfm Upvote 0 Downvote
I suppose this is 22V, K31835. It is covered by ASME SA-336, 541, 542 and 832. Look them up and which scope covers your product size. = = = = = = = = = = = = = = = = = = = = Rust never sleeps Neither should your protection http://www.trent-tube.com/contact/Tech_Assist.cfm
Jun 27, 2007 #3 ijzer Materials Joined Oct 25, 2002 Messages 313 Location NL Forgings: A 182/ A 336 Grade F22V/A 541 Grade 22V Plate A 542 Type D cl. 4a / A 832 Grade 22V Upvote 0 Downvote