What are the ASTM/ASME specification numbers for 2.25Cr-1Mo-0.25V pressure vessel steel for heavy wall reactors?
 
Forgings: A 182/ A 336 Grade F22V/A 541 Grade 22V
Plate A 542 Type D cl. 4a / A 832 Grade 22V
 