writing a program for cooling of lubricating oil used in natural gas engines and compressors. Any web site showing the specific heat as a function of viscousity and temperature?
thanks
 
hi
the back of any heat transfer book has to have an appendix of fluid properties as functions of temperature.
but, that aside ...light oil at 150F , Cp = .48 BTU/lbm/F (per Kreith, Table A-3)

daveleo
 
Heat Transfer by J.P.Holman, Table A-4, gives for an unused engine oil the following data:

t,oC Cp, kJ/(kg.K)

0 1.796
20 1.880
40 1.964
60 2.047
80 2.131
100 2.219
120 2.307
140 2.395
160 2.483

It also provide viscosities and othe relevant thermophysical properties. [smile]
 
For mineral oils, Cp, kJ/(kg.oC)

Cp = (1.69+0.0034t)d-0.5

where t is in deg C, and d is density of the oil at 20 deg C.

Common Cp values at 20 deg C:

Polyhydric alcohols, 2.43; petroleum oils, 1.88; silicones, 1.47. [pipe]
 