Aug 23, 2010 #1 dcopps Mechanical Joined Feb 8, 2005 Messages 70 Location US I am seeking variations in the constant-pressure specific heat capacity up to the boiling point for Lanthanum (La) and Cerium (Ce). I understand this value varies a good bit with temperature, so am looking for a plot of some kind.
I am seeking variations in the constant-pressure specific heat capacity up to the boiling point for Lanthanum (La) and Cerium (Ce). I understand this value varies a good bit with temperature, so am looking for a plot of some kind.
Sep 5, 2010 #2 Arpene Chemical Joined Sep 2, 2010 Messages 7 Location IL Hi Well these data are from Perry's handbook. Unfortunatly they don't go pretty much in the near of the boiling point. la(273–1009) CP=5.91 + 0.00100T cal/(molK) Ce (273K–908K) CP=5.88 + 0.00123T cal/(molK) Upvote 0 Downvote