I am seeking variations in the constant-pressure specific heat capacity up to the boiling point for Lanthanum (La) and Cerium (Ce). I understand this value varies a good bit with temperature, so am looking for a plot of some kind.
 
Hi

Well these data are from Perry's handbook. Unfortunatly they don't go pretty much in the near of the boiling point.

la(273–1009)

CP=5.91 + 0.00100T cal/(molK)

Ce (273K–908K)

CP=5.88 + 0.00123T cal/(molK)

 