Bioengineer
Aug 17, 2012
1
I'm trying to source a specific braid pattern (.001 in x .005 in, 304V SS 300 kpsi, 30 PPI) and have yet to find a source. I'd like to stay clear of a custom run. Any suggestions?
 
Replies continue below

Recommended for you

I don't quite understand your teminology for what you want.

That said, I know of a guy who makes a product that includes a tubular braid of stainless wire, which he gets by the simple expedient of stripping the hose out of braided fuel hose.