I am looking for a manufacturer of General Motors specification 436 stainless steel.
Any help given would be greatly appreciated.

Thanks,
Afterhrs
 
In addition to those two, some of the best 436 was the product imported from France, from Ugine, now called Accelor.
 
mcguire is a stainless steel expert, so you should definitely follow-up on his suggestion. However, there is a typographical error in the company name. It should read ARCELOR not Accelor. You can obtain more information on ARCELOR and UGINE by using the following links:



 
I would like to thank all that replied for your help!

Kind regards,