I am looking for suppliers of round bar material under the following names - Nitronic 32, XM-28, UNS S24100, and Carpenter 18Cr-2Ni-12Mn. So far I have only located Carpenter as a source for round bar. Can anyone provide me with alternative sources?

Pete
 
JT Ryerson?


The contact I work with is very helpful and they always seem to have what I want, and it is usually here in the next day or so.
 
Ryerson doesn't carry it according to their site. We use them for other materials.
 